General
Property | Value | Temperature |
---|---|---|
Density | 8.8 g/cm³ Show Material materials with Density of 8.8 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 120 GPa Show Material materials with Elastic modulus of 120 GPa at 23.0 °C | 23.0 °C | |
Elongation | 3 % Show Material materials with Elongation of 3 % at 23.0 °C | 23.0 °C | |
Shear modulus | 40 GPa Show Material materials with Shear modulus of 40 GPa at 23.0 °C | 23.0 °C | Typical for Wrought Copper Brass |
Tensile strength | 500 MPa Show Material materials with Tensile strength of 500 MPa at 23.0 °C | 23.0 °C | |
Yield strength | 430 MPa Show Material materials with Yield strength of 430 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 1020 °C Show Material materials with Melting point of 1020 °C | |
Specific heat capacity | 380 J/(kg·K) Show Material materials with Specific heat capacity of 380 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 190 W/(m·K) Show Material materials with Thermal conductivity of 190 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 89 - 91 % | |
Iron | 0 - 0.05 % | |
Lead | 0 - 0.05 % | |
Other | 0 - 0.2 % | |
Zinc | 8.7 - 11 % |