General
Property | Value | Temperature |
---|---|---|
Density | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 1080 °C Show Material materials with Melting point of 1080 °C | |
Specific heat capacity | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 260 W/(m·K) Show Material materials with Thermal conductivity of 260 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 96.8 - 97.8 % | |
Iron | 2.1 - 2.6 % | |
Lead | 0 - 0.03 % | |
Other | 0 - 0.2 % | |
Phosphorus | 0.02 - 0.15 % | |
Zinc | 0.05 - 0.2 % |