UNS C26000 H10

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 GPa

Show Material materials with Elastic modulus of 110 GPa

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Tensile strength

23.0 °C

680 MPa

Show Material materials with Tensile strength of 680 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2E-5 1/K

Melting point

920 °C

Show Material materials with Melting point of 920 °C

Specific heat capacity

23.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

Thermal conductivity

23.0 °C

120 W/(m·K)

Show Material materials with Thermal conductivity of 120 W/(m·K)

Chemical properties

PropertyValue

Bismuth

0 - 5.9E-3 %

Show Material materials with Bismuth of 0 - 5.9E-3 %

Copper

68.5 - 71.5 %

Show Material materials with Copper of 68.5 - 71.5 %

Iron

0 - 0.05 %

Show Material materials with Iron of 0 - 0.05 %

Lead

0 - 0.07 %

Show Material materials with Lead of 0 - 0.07 %

Other

0 - 0.3 %

Show Material materials with Other of 0 - 0.3 %

Zinc

28.1 - 31.5 %

Show Material materials with Zinc of 28.1 - 31.5 %