See where UNS C51000 H10 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.8 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.8E-5 1/K at 23 °C
Melting point
Tm960 °C
Specific heat capacity
cp380 J/(kg·K) at 23 °C
Thermal conductivity
λ77 W/(m·K) at 23 °C
Element
Weight %
Comment
92.9 - 95.5 %
4.5 - 5.8 %
0.03 - 0.35 %
0 - 0.1 %
0 - 0.05 %