UNS C70600 H55

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.9 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

140 GPa at 23 °C

Show Wrought Copper Nickel Grade materials with Elastic modulus of 140 GPa at 23 °C

Tensile strength

Rm

360 MPa at 23 °C

Show Wrought Copper Nickel Grade materials with Tensile strength of 360 MPa at 23 °C

Yield strength

YS

280 MPa at 23 °C

Show Wrought Copper Nickel Grade materials with Yield strength of 280 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.7E-5 1/K at 23 °C

Melting point

Tm

1100 °C

Specific heat capacity

cp

380 J/(kg·K) at 23 °C

Thermal conductivity

λ

44 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Cu

84.7 - 90 %

Ni

9 - 11 %

Fe

1 - 1.8 %

Pb

0 - 0.05 %

Mn

0 - 1 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.