UNS R30035 Hot Forged

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.7 g/cm³

Show Material materials with Density of 8.7 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

230 GPa

Show Material materials with Elastic modulus of 230 GPa

Tensile strength

23.0 °C

1200 MPa

Show Material materials with Tensile strength of 1200 MPa

Yield strength

23.0 °C

980 MPa

Show Material materials with Yield strength of 980 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

Melting point

1320 °C

Show Material materials with Melting point of 1320 °C

Specific heat capacity

23.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

23.0 °C

11 W/(m·K)

Show Material materials with Thermal conductivity of 11 W/(m·K)

Chemical properties

PropertyValue

Boron

0 - 0.015 %

Show Material materials with Boron of 0 - 0.015 %

Carbon

0 - 0.025 %

Show Material materials with Carbon of 0 - 0.025 %

Chromium

19 - 21 %

Show Material materials with Chromium of 19 - 21 %

Cobalt

29.1 - 39 %

Show Material materials with Cobalt of 29.1 - 39 %

Iron

0 - 1 %

Show Material materials with Iron of 0 - 1 %

Manganese

0 - 0.15 %

Show Material materials with Manganese of 0 - 0.15 %

Molybdenum

9 - 10.5 %

Show Material materials with Molybdenum of 9 - 10.5 %

Nickel

33 - 37 %

Show Material materials with Nickel of 33 - 37 %

Phosphorus

0 - 0.02 %

Show Material materials with Phosphorus of 0 - 0.02 %

Silicon

0 - 0.15 %

Show Material materials with Silicon of 0 - 0.15 %

Sulfur

0 - 0.01 %

Show Material materials with Sulfur of 0 - 0.01 %

Titanium

0 - 1 %

Show Material materials with Titanium of 0 - 1 %