General
Property | Value | Temperature |
---|---|---|
Density | 7.8 g/cm³ Show Supplier Material materials with Density of 7.8 g/cm³ at 23.0 °C | 23.0 °C |
Dimension
Property | Value |
---|---|
Inside diameter | 400 - 730 mm Show Supplier Material materials with Inside diameter of 400 - 730 mm |
Length | 1750 - 3370 mm Show Supplier Material materials with Length of 1750 - 3370 mm |
Outside diameter | 450 - 910 mm Show Supplier Material materials with Outside diameter of 450 - 910 mm |
Thickness | 150 - 230 mm Show Supplier Material materials with Thickness of 150 - 230 mm |
Width | 1350 - 2540 mm Show Supplier Material materials with Width of 1350 - 2540 mm |
Chemical properties
Property | ||
---|---|---|
Carbon | 0.5 - 0.6 % | |
Chromium | 0.5 - 0.8 % | |
Copper | 0 - 0.3 % | |
Iron | Balance | |
Manganese | 0.5 - 0.8 % | |
Molybdenum | 0.15 - 0.3 % | |
Nickel | 1.4 - 1.8 % | |
Phosphorus | 0 - 0.03 % | |
Silicon | 0.1 - 0.4 % | |
Sulfur | 0 - 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | Steel forgings are applied for manufacture of the details of machinery and spare parts for metallurgical, mining and machine-building equipment. | |
Processing methods | Manufactured by open die forging |