General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.89 g/cm³ Show Supplier Material materials with Density of 0.89 g/cm³ at 20.0 °C | 20.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 623 % Show Supplier Material materials with Elongation of 623 % at 20.0 °C | 20.0 °C | ASTM D412 |
Hardness, Shore A | 10 [-] Show Supplier Material materials with Hardness, Shore A of 10 [-] at 20.0 °C | 20.0 °C | ASTM D2240 |
Modulus at 100% elongation | 0.5 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.5 GPa at 20.0 °C | 20.0 °C | ASTM D412 |
Tear strength | 5.78 kN/m Show Supplier Material materials with Tear strength of 5.78 kN/m at 20.0 °C | 20.0 °C | ASTM D624 |
Tensile strength | 1.6 MPa Show Supplier Material materials with Tensile strength of 1.6 MPa at 20.0 °C | 20.0 °C | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Elastocon® 2810 is FDA compliant and well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics and resilience. | |
Other | Elastocon® 2810 thermoplastic elastomer compound does not require drying. Elastocon® thermoplastic elastomers are not compatible with flexible PVC and should not be blended with or used in an application where direct contact is intended. It can be overmolded onto polypropylene. | |
Processing methods | Injection molding, extrusion, blow molding. |