General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.88 g/cm³ Show Supplier Material materials with Density of 0.88 g/cm³ at 20.0 °C | 20.0 °C | ASTM D792 |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 543 % Show Supplier Material materials with Elongation of 543 % at 20.0 °C | 20.0 °C | ASTM D412 |
Hardness, Shore A | 25 [-] Show Supplier Material materials with Hardness, Shore A of 25 [-] at 20.0 °C | 20.0 °C | ASTM D2240 |
Modulus at 100% elongation | 0.74 GPa Show Supplier Material materials with Modulus at 100% elongation of 0.74 GPa at 20.0 °C | 20.0 °C | ASTM D412 |
Tear strength | 9.82 kN/m Show Supplier Material materials with Tear strength of 9.82 kN/m at 20.0 °C | 20.0 °C | ASTM D624 |
Tensile strength | 2.4 MPa Show Supplier Material materials with Tensile strength of 2.4 MPa at 20.0 °C | 20.0 °C | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Elastocon® 2825PE is FDA compliant and well suited for consumer goods and industrial applications requiring UV stability. | |
Other | Elastocon® 2825PE thermoplastic elastomer compound does not require drying. Elastocon® thermoplastic elastomers are not compatible with flexible PVC and should not be blended with or used in an application where direct contact is intended. It can be overmolded and coextruded with polyethylene. | |
Processing methods | Injection molding, extrusion, blow molding. |