Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.8 g/cm³ Show Supplier Material materials with Density of 8.8 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 135 GPa Show Supplier Material materials with Elastic modulus of 135 GPa |
Elongation A5 | 23.0 °C | 20 % Show Supplier Material materials with Elongation A5 of 20 % |
Hardness, Brinell | 23.0 °C | 180 [-] Show Supplier Material materials with Hardness, Brinell of 180 [-] |
Tensile strength | 23.0 °C | 650 MPa Show Supplier Material materials with Tensile strength of 650 MPa |
Yield strength Rp0.2 | 23.0 °C | 500 MPa Show Supplier Material materials with Yield strength Rp0.2 of 500 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K |
Thermal conductivity | 23.0 °C | 239 W/(m·K) Show Supplier Material materials with Thermal conductivity of 239 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 2.50E+7 S/m Show Supplier Material materials with Electrical conductivity of 2.50E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.2 % Show Supplier Material materials with Aluminium of 0 - 0.2 % |
Beryllium | 0.4 - 0.7 % Show Supplier Material materials with Beryllium of 0.4 - 0.7 % |
Cobalt | 2.4 - 2.7 % Show Supplier Material materials with Cobalt of 2.4 - 2.7 % |
Copper | 95.6 - 97.2 % Show Supplier Material materials with Copper of 95.6 - 97.2 % |
Iron | 0 - 0.1 % Show Supplier Material materials with Iron of 0 - 0.1 % |
Other | 0 - 0.5 % Show Supplier Material materials with Other of 0 - 0.5 % |
Silicon | 0 - 0.2 % Show Supplier Material materials with Silicon of 0 - 0.2 % |
Do you have a technical question or need more information about this material?