General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Density of 8.3 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 135 GPa Show Supplier Material materials with Elastic modulus of 135 GPa |
Elongation A5 | 23.0 °C | 3 % Show Supplier Material materials with Elongation A5 of 3 % |
Hardness, Brinell | 23.0 °C | 340 [-] Show Supplier Material materials with Hardness, Brinell of 340 [-] |
Tensile strength | 23.0 °C | 1150 MPa Show Supplier Material materials with Tensile strength of 1150 MPa |
Yield strength Rp0.2 | 23.0 °C | 1100 MPa Show Supplier Material materials with Yield strength Rp0.2 of 1100 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.7E-5 1/K |
Thermal conductivity | 23.0 °C | 125 W/(m·K) Show Supplier Material materials with Thermal conductivity of 125 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.20E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.20E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.2 % Show Supplier Material materials with Aluminium of 0 - 0.2 % |
Beryllium | 1.8 - 2 % Show Supplier Material materials with Beryllium of 1.8 - 2 % |
Copper | 96.1 - 98 % Show Supplier Material materials with Copper of 96.1 - 98 % |
Iron | 0 - 0.4 % Show Supplier Material materials with Iron of 0 - 0.4 % |
Nickel | 0.2 - 0.6 % Show Supplier Material materials with Nickel of 0.2 - 0.6 % |
Other | 0 - 0.5 % Show Supplier Material materials with Other of 0 - 0.5 % |
Silicon | 0 - 0.2 % Show Supplier Material materials with Silicon of 0 - 0.2 % |