Titanium wire SM

Alternative and trade names
Titanium Wire
Want to keep this datasheet? Save it now in your required format

Description

Titanium wire is drawn from forged rods. Quality control process is according to ASTM grades of titanium to ensure no contamination.

Related Standards

This material data has been provided by Stanford Advanced Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

4.54 g/cm³

Show Supplier Material materials with Density of 4.54 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

116 GPa

Show Supplier Material materials with Elastic modulus of 116 GPa

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

Hardness, Brinell

23.0 °C

120 [-]

Show Supplier Material materials with Hardness, Brinell of 120 [-]

Tensile strength

23.0 °C

240 MPa

Show Supplier Material materials with Tensile strength of 240 MPa

Yield strength

23.0 °C

170 - 310 MPa

Show Supplier Material materials with Yield strength of 170 - 310 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

8.6E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8.6E-6 1/K

Melting point

1668 °C

Show Supplier Material materials with Melting point of 1668 °C

Thermal conductivity

23.0 °C

21.9 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 21.9 W/(m·K)

Technological properties

Property
Application areas

Welding wires, MMO Wire Anodes, Racks, Glass frames

Chemical composition

Purity of 99.99%

Processing history

It is drawn from forged rods. SAM operates a strict quality control process using ASTM grades of titanium to ensure no contamination.