Nontoxic and tasteless white powder with stable chemical properties. Yittria stabilized zirconia oxide’s special surface and median grain diameter can be controlled to customer’s demand. The different properties of Zirconia powders, such as the grade of jet and prilled powder can be made for the customer’s requirement.

This material data has been provided by Zhengzhou Sky Universe Trade Co.,LTD..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size D50

0.4 - 0.8 μm

Show Supplier Material materials with Particle size D50 of 0.4 - 0.8 μm

Specific surface area

12 - 17 m²/g

Show Supplier Material materials with Specific surface area of 12 - 17 m²/g

measured with the BET-method

Chemical properties

PropertyValueComment

Aluminium

0.01 %

Show Supplier Material materials with Aluminium of 0.01 %

Al₂O₃

Chlorine

0.03 - 0.08 %

Show Supplier Material materials with Chlorine of 0.03 - 0.08 %

Iron

3E-3 %

Show Supplier Material materials with Iron of 3E-3 %

Fe₂O₃

Silicon

0.02 %

Show Supplier Material materials with Silicon of 0.02 %

SiO₂

Sodium

0.01 %

Show Supplier Material materials with Sodium of 0.01 %

Na₂O

Titanium

0.01 %

Show Supplier Material materials with Titanium of 0.01 %

TiO₂

Zirconium

99.9 %

Show Supplier Material materials with Zirconium of 99.9 %

ZrO₂, minimum

Technological properties

Property
Application areas

YSZ powder is suitable for production of different structure ceramics,electronic ceramics,biological ceramics,advanced refractory,optical communication device,man-made jewelry,sensor ,solid fuel battery,grinding and polish trade and so on. Structural Ceramics: since nano ZrO2 ceramics with high toughness, high flexural strength and high wear resistance, excellent thermal insulation properties, thermal expansion coefficient close to steel, etc., nano ZrO2 powder is widely used in the field of structural ceramics.