Description

Super Duplex UNS S32750 is the most common super duplex grade in the market. UNS S32750 is a duplex stainless steel especially designed for service in aggressive chloride-containing environments with high mechanical strength.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

16 - 406.4 mm

Show Supplier Material materials with Diameter of 16 - 406.4 mm

Mechanical

PropertyTemperatureValue

Charpy impact energy, V-notch

-46.0 °C

45 J

Show Supplier Material materials with Charpy impact energy, V-notch of 45 J

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

Hardness, Brinell

23.0 °C

310 [-]

Show Supplier Material materials with Hardness, Brinell of 310 [-]

Tensile strength

23.0 °C

750 MPa

Show Supplier Material materials with Tensile strength of 750 MPa

Yield strength Rp0.2

23.0 °C

550 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 550 MPa

Chemical properties

PropertyValue

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

Chromium

24 - 26 %

Show Supplier Material materials with Chromium of 24 - 26 %

Copper

0.5 %

Show Supplier Material materials with Copper of 0.5 %

Iron

Balance

Manganese

1.2 %

Show Supplier Material materials with Manganese of 1.2 %

Molybdenum

3 - 5 %

Show Supplier Material materials with Molybdenum of 3 - 5 %

Nickel

6 - 8 %

Show Supplier Material materials with Nickel of 6 - 8 %

Nitrogen

0.24 - 0.32 %

Show Supplier Material materials with Nitrogen of 0.24 - 0.32 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

0.8 %

Show Supplier Material materials with Silicon of 0.8 %

Sulfur

0.02 %

Show Supplier Material materials with Sulfur of 0.02 %

Technological properties

Property
Application areas

It is widely used in oil & gas, hydropower, pressure vessels, pulp & paper, structural components and chemical tankers.

Corrosion properties

High resistance to stress corrosion cracking in halide containing environments, High resistance to pitting and crevice corrosion, High resistance to general corrosion, High resistance to erosion corrosion and corrosion fatigue. PREN ≥ 40

Heat Treatment

Solution annealing at 1100°C followed by water quenching.

Welding

Very good