Chemical properties
Property | Value | Comment |
---|---|---|
Carbon | 0.15 % Show Supplier Material materials with Carbon of 0.15 % | max. |
Chromium | 0.15 % Show Supplier Material materials with Chromium of 0.15 % | max. |
Copper | 0.2 % Show Supplier Material materials with Copper of 0.2 % | max. |
Manganese | 1.65 % Show Supplier Material materials with Manganese of 1.65 % | max. |
Molybdenum | 0.16 % Show Supplier Material materials with Molybdenum of 0.16 % | max. |
Nickel | 0.2 % Show Supplier Material materials with Nickel of 0.2 % | max. |
Other | 0.005 % Show Supplier Material materials with Other of 0.005 % | min. Cb/Nb |
Phosphorus | 0.02 % Show Supplier Material materials with Phosphorus of 0.02 % | max. |
Sulfur | 0.025 % Show Supplier Material materials with Sulfur of 0.025 % | max. |
Titanium | 0.005 % Show Supplier Material materials with Titanium of 0.005 % | min. |
Vanadium | 0.005 % Show Supplier Material materials with Vanadium of 0.005 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | Battery components: cans, covers, connector strips | |
Other | ||
Packaging size | ||
Surface Finish | ||
Surface protection |