General
Property | Value |
---|---|
Bulk density | 2.47 - 2.54 g/cm³ Show Supplier Material materials with Bulk density of 2.47 - 2.54 g/cm³ |
Particle size D10 | 20.0 - 25.0 μm Show Supplier Material materials with Particle size D10 of 20.0 - 25.0 μm |
Particle size D50 | 32.0 - 35.0 μm Show Supplier Material materials with Particle size D50 of 32.0 - 35.0 μm |
Particle size D90 | 42.0 - 45.0 μm Show Supplier Material materials with Particle size D90 of 42.0 - 45.0 μm |
Rheological Properties
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Supplier Material materials with Aluminium of 5.5 - 6.5 % | ||
Carbon | 0.08 % Show Supplier Material materials with Carbon of 0.08 % | Maximum | |
Hydrogen | 0.0125 % Show Supplier Material materials with Hydrogen of 0.0125 % | ||
Iron | 0.25 % Show Supplier Material materials with Iron of 0.25 % | ||
Nitrogen | 0.03 % Show Supplier Material materials with Nitrogen of 0.03 % | ||
Other | 0.4 % Show Supplier Material materials with Other of 0.4 % | Total Maximum | |
Oxygen | 0.13 % Show Supplier Material materials with Oxygen of 0.13 % | ||
Titanium | Balance | ||
Vanadium | 3.5 - 4.5 % Show Supplier Material materials with Vanadium of 3.5 - 4.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing, Metal Injection Molding, Thermal Spray, Biomedical, Aerospace |