General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.85 g/cm³ Show Supplier Material materials with Density of 7.85 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 17 % Show Supplier Material materials with Elongation of 17 % |
Tensile strength | 23.0 °C | 485 - 620 MPa Show Supplier Material materials with Tensile strength of 485 - 620 MPa |
Yield strength | 23.0 °C | 260 MPa Show Supplier Material materials with Yield strength of 260 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.27 % Show Supplier Material materials with Carbon of 0.27 % |
Manganese | 0.85 - 1.2 % Show Supplier Material materials with Manganese of 0.85 - 1.2 % |
Phosphorus | 0.04 % Show Supplier Material materials with Phosphorus of 0.04 % |
Silicon | 0.15 - 0.4 % Show Supplier Material materials with Silicon of 0.15 - 0.4 % |
Sulfur | 0.035 % Show Supplier Material materials with Sulfur of 0.035 % |
Technological properties
Property | ||
---|---|---|
Application areas | Boiler & Pressure Vessel Building |