ASTM A516 Grade 70

Want to keep this datasheet? Save it now in your required format

Description

TJC Steel can supply A516 Grade 70/ A516 Gr70 pressure vessel steel plate, mainly used in construction for pressure vessels.

Related Standards

Equivalent Materials

This material data has been provided by TJC Iron & Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.85 g/cm³

Show Supplier Material materials with Density of 7.85 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

17 %

Show Supplier Material materials with Elongation of 17 %

Tensile strength

23.0 °C

485 - 620 MPa

Show Supplier Material materials with Tensile strength of 485 - 620 MPa

Yield strength

23.0 °C

260 MPa

Show Supplier Material materials with Yield strength of 260 MPa

Chemical properties

PropertyValue

Carbon

0.27 %

Show Supplier Material materials with Carbon of 0.27 %

Manganese

0.85 - 1.2 %

Show Supplier Material materials with Manganese of 0.85 - 1.2 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

0.15 - 0.4 %

Show Supplier Material materials with Silicon of 0.15 - 0.4 %

Sulfur

0.035 %

Show Supplier Material materials with Sulfur of 0.035 %

Technological properties

Property
Application areas

Boiler & Pressure Vessel Building