TJC Steel can supply A588 Grade A/ A588 GrA High-Strength Low-Alloy Structural Steel Plate, mainly used in many applications in the bare condition.

Related Standards

Equivalent Materials

This material data has been provided by TJC Iron & Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.85 g/cm³

Show Supplier Material materials with Density of 7.85 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

21 %

Show Supplier Material materials with Elongation of 21 %

Tensile strength

23.0 °C

485 MPa

Show Supplier Material materials with Tensile strength of 485 MPa

Yield strength

23.0 °C

345 MPa

Show Supplier Material materials with Yield strength of 345 MPa

Chemical properties

PropertyValue

Carbon

0.19 %

Show Supplier Material materials with Carbon of 0.19 %

Manganese

0.8 - 1.25 %

Show Supplier Material materials with Manganese of 0.8 - 1.25 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

0.3 - 0.65 %

Show Supplier Material materials with Silicon of 0.3 - 0.65 %

Sulfur

0.05 %

Show Supplier Material materials with Sulfur of 0.05 %

Technological properties

Property
Application areas

Structural Anti-Corrosion Building