Low Density Polyethylene (LD PE) for Film Applications

.XLSX
.PDF
Save

Description

Recycled low density polyethylene granulate for film applications. In addition to the standard reclaimed polymer portfolio, WELA Plast offers individually optimized customer specific formulations, especially when it comes to customized product colors and property profiles.

Properties

General

Ash content cash

1 - 5 % at 625 °C

DIN EN ISO 3451-1:1997

Density ρ

0.92 - 0.98 g/cm³ at 20 °C

DIN EN ISO 1183-1

Melt mass-flow rate MFR

0.1 - 3.5 g/10min at 190 °C

DIN EN ISO 1133-1 (190°C/2.16kg)

Technological properties

Application areas

Carrying bags, waste bags, mailing bags, agricultural film

Color

Natural, white, black, blue, yellow, jazz, opaque

This material data has been provided by Wela Plast.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.