General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 20.0 °C | 4.505 g/cm³ Show Material materials with Density of 4.505 g/cm³ | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 20.0 °C | 108.0 GPa Show Material materials with Elastic modulus of 108.0 GPa | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | |
200.0 °C | 95.0 GPa Show Material materials with Elastic modulus of 95.0 GPa | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | ||
400.0 °C | 82.0 GPa Show Material materials with Elastic modulus of 82.0 GPa | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | ||
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium | ||||
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||||
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium | ||||
Specific heat capacity | 20.0 °C | 520.0 J/(kg·K) Show Material materials with Specific heat capacity of 520.0 J/(kg·K) | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | |
200.0 °C | 570.0 J/(kg·K) Show Material materials with Specific heat capacity of 570.0 J/(kg·K) | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | ||
400.0 °C | 630.0 J/(kg·K) Show Material materials with Specific heat capacity of 630.0 J/(kg·K) | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | ||
Thermal conductivity | 20.0 °C | 22.6 W/(m·K) Show Material materials with Thermal conductivity of 22.6 W/(m·K) | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | |
200.0 °C | 20.9 W/(m·K) Show Material materials with Thermal conductivity of 20.9 W/(m·K) | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | ||
400.0 °C | 19.3 W/(m·K) Show Material materials with Thermal conductivity of 19.3 W/(m·K) | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Electrical resistivity | 20.0 °C | 4.7e-07 Ω·m Show Material materials with Electrical resistivity of 4.7e-07 Ω·m | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat |
200.0 °C | 8.2e-07 Ω·m Show Material materials with Electrical resistivity of 8.2e-07 Ω·m | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat | |
400.0 °C | 1.18e-06 Ω·m Show Material materials with Electrical resistivity of 1.18e-06 Ω·m | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.06 Show Material materials with Carbon of 0.06 | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat |
Hydrogen | 0.013 Show Material materials with Hydrogen of 0.013 | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat |
Iron | 0.15 Show Material materials with Iron of 0.15 | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Flat, Tube |
0.2 Show Material materials with Iron of 0.2 | Welded | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Tube | |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Tube, Flat |
Oxygen | 0.12 Show Material materials with Oxygen of 0.12 | Welded | VdTÜV WB 230-3, DIN 17850, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Forging, Rod, Wire, Flat, Tube |
0.18 Show Material materials with Oxygen of 0.18 | Welded | DIN 17850, VdTÜV WB 230-3, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-2, DIN 17862, DIN 17864, DIN 17860 | Tube | |
Titanium | 99.1 % Show Material materials with Titanium of 99.1 % | Welded | DIN 17850, VdTÜV WB 230-2, WL 3.7024-1, VdTÜV WB 230-1, VdTÜV WB 230-3, DIN 17862, DIN 17864, DIN 17860 | Tube |
99.2 % Show Material materials with Titanium of 99.2 % | Welded | DIN 17850 | Flat, Tube, Forging, Rod, Wire |