Polymer Silicon Carbide Composite SICAPRINT™ P100

Polymer Silicon Carbide Composite SICAPRINT™ P200

Polymer Silicon Carbide Composite SICAPRINT™ P210

Search results

Materials

Available properties

General

Density (g/cm³)

Mechanical

Elastic modulus (GPa)
Hardness, Shore D ([-])
Flexural strength (MPa)
Compressive strength (MPa)

Thermal

Thermal conductivity (W/(m·K))

You should select at least 1 property to see the chart!

Polymer Silicon Carbide Composite SICAPRINT™ P100

Polymer Silicon Carbide Composite SICAPRINT™ P200

Polymer Silicon Carbide Composite SICAPRINT™ P210

Primary standard name

Equivalent standard names

Related standards

Chemical composition

Element

Weight %

Comment

Element

Weight %

Comment

Element

Weight %

Comment

Material Information

Secondary Phase

Mechanical

Elastic modulus, E

19 GPa at 23 °C

13 GPa at 23 °C

17 GPa at 23 °C

Hardness, Shore D, HS D

90 [-] at 23 °C

90 [-] at 23 °C

90 [-] at 23 °C

Flexural strength, σbend

55 MPa at 23 °C

95 MPa at 23 °C

120 MPa at 23 °C

Compressive strength, Rmc

130 MPa at 23 °C

120 MPa at 23 °C

140 MPa at 23 °C

General

Density, ρ

2 g/cm³ at 23 °C

2 g/cm³ at 23 °C

2 g/cm³ at 23 °C

Thermal

Thermal conductivity, λ

2.6 W/(m·K) at 23 °C

2.4 W/(m·K) at 23 °C

2.4 W/(m·K) at 23 °C