Polymer Silicon Carbide Composite SICAPRINT™ P100

Want to keep this datasheet? Save it now in your required format

Description

Pragmatic solution for functional parts that are exposed to abrasive and corrosive fluids and constant temperatures up to 200 °C. The simple refinement process allows for economical solutions.


Depending on the technical requirements a variety of resins is being held on demand to realize the desired result.


The advantages of SICAPRINT™ are:

  • Abrasion resistance
  • Corrosion resistance
  • Economically advantageous

This material data has been provided by SGL Carbon.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

2 g/cm³

Show Supplier Material materials with Density of 2 g/cm³

Mechanical

PropertyValue

Compressive strength

130 MPa

Show Supplier Material materials with Compressive strength of 130 MPa

Elastic modulus

19 GPa

Show Supplier Material materials with Elastic modulus of 19 GPa

Flexural strength

55 MPa

Show Supplier Material materials with Flexural strength of 55 MPa

Hardness, Shore D

90.0 [-]

Show Supplier Material materials with Hardness, Shore D of 90.0 [-]

Thermal

PropertyValue

Thermal conductivity

2.6 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 2.6 W/(m·K)

Technological properties

Property