General
Property | Value | Temperature |
---|---|---|
Density | 2 g/cm³ Show Supplier Material materials with Density of 2 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature |
---|---|---|
Compressive strength | 120 MPa Show Supplier Material materials with Compressive strength of 120 MPa at 23.0 °C | 23.0 °C |
Elastic modulus | 13 GPa Show Supplier Material materials with Elastic modulus of 13 GPa at 23.0 °C | 23.0 °C |
Flexural strength | 95 MPa Show Supplier Material materials with Flexural strength of 95 MPa at 23.0 °C | 23.0 °C |
Hardness, Shore D | 90 [-] Show Supplier Material materials with Hardness, Shore D of 90 [-] at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Thermal conductivity | 2.4 W/(m·K) Show Supplier Material materials with Thermal conductivity of 2.4 W/(m·K) at 23.0 °C | 23.0 °C |
Technological properties
Property |
---|