Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Polymer Silicon Carbide Composite SICAPRINT™ P210
Pragmatic solution for functional parts that are exposed to abrasive and corrosive fluids and constant temperatures up to 200 °C. The simple refinement process allows for economical solutions.
Depending on the technical requirements a variety of resins is being held on demand to realize the desired result.
The advantages of SICAPRINT™ are:
This material data has been provided by SGL Carbon.
See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
All categories
General
Property | Value |
---|---|
Density | 2 g/cm³ Show Supplier Material materials with Density of 2 g/cm³ |
Mechanical
Property | Value |
---|---|
Compressive strength | 140 MPa Show Supplier Material materials with Compressive strength of 140 MPa |
Elastic modulus | 17 GPa Show Supplier Material materials with Elastic modulus of 17 GPa |
Flexural strength | 120 MPa Show Supplier Material materials with Flexural strength of 120 MPa |
Hardness, Shore D | 90.0 [-] Show Supplier Material materials with Hardness, Shore D of 90.0 [-] |
Thermal
Property | Value |
---|---|
Thermal conductivity | 2.4 W/(m·K) Show Supplier Material materials with Thermal conductivity of 2.4 W/(m·K) |
Technological properties
Property |
---|
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2022 Matmatch GmbH, All rights reserved.
Made with ❤️ in Munich!