Chrom: 2 %

Quick Comparison

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type A Class 2 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type D Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type A Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type B Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade AQ47

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade DQ47

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade EQ47

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade EQ51

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade FQ51

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade EQ70

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade FQ70

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade AQ51

Geliefert von:

1 Matmatch-Lieferant

Kohlenstoffarmer Stahl

ABS Grade DQ51

Geliefert von:

1 Matmatch-Lieferant

Seite 1 von 10