General
Property | Value | Comment |
---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Elongation | 11.5 % Show Material materials with Elongation of 11.5 % | Predicted Value, A200 | |||
13 % Show Material materials with Elongation of 13 % | Quenched and Tempered | ASTM A542 | Plate | A50 | |
16.0 % Show Material materials with Elongation of 16.0 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Elongation of 18.4 % | Predicted Value, Transverse | ||||
19.4 % Show Material materials with Elongation of 19.4 % | Predicted Value | ||||
20.2 % Show Material materials with Elongation of 20.2 % | Predicted Value, A80 Transverse | ||||
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Reduction of area | 41.1 % Show Material materials with Reduction of area of 41.1 % | Predicted Value | |||
45.1 % Show Material materials with Reduction of area of 45.1 % | Predicted Value, Transverse | ||||
Shear modulus | 80 GPa Show Material materials with Shear modulus of 80 GPa | Predicted Value | |||
Shear strength | 616.7 MPa Show Material materials with Shear strength of 616.7 MPa | Predicted Value | |||
Tensile strength | 795 - 930 MPa Show Material materials with Tensile strength of 795 - 930 MPa | Quenched and Tempered | ASTM A542 | Plate | |
Yield strength | 310.9 MPa Show Material materials with Yield strength of 310.9 MPa | Predicted Value, RP1 | |||
330.2 MPa Show Material materials with Yield strength of 330.2 MPa | Predicted Value, RP1 Transverse | ||||
363.4 MPa Show Material materials with Yield strength of 363.4 MPa | Predicted Value, RP05 | ||||
491.6 MPa Show Material materials with Yield strength of 491.6 MPa | Predicted Value, RP02 Transverse | ||||
516.2 MPa Show Material materials with Yield strength of 516.2 MPa | Predicted Value, Transverse | ||||
657.2 MPa Show Material materials with Yield strength of 657.2 MPa | Predicted Value, RP02 | ||||
690 MPa Show Material materials with Yield strength of 690 MPa | Quenched and Tempered | ASTM A542 | Plate | ||
768 MPa Show Material materials with Yield strength of 768 MPa | Predicted Value, RP002 |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.1e-05 - 1.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Specific heat capacity | 448 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Thermal conductivity | 36 - 43 W/(m·K) Show Material materials with Thermal conductivity of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.15 % Show Material materials with Carbon of 0.15 % | Quenched and Tempered | ASTM A542 | Plate |
Chromium | 2 - 2.5 % Show Material materials with Chromium of 2 - 2.5 % | Quenched and Tempered | ASTM A542 | Plate |
Copper | 0.4 % Show Material materials with Copper of 0.4 % | Quenched and Tempered | ASTM A542 | Plate |
Manganese | 0.3 - 0.6 % Show Material materials with Manganese of 0.3 - 0.6 % | Quenched and Tempered | ASTM A542 | Plate |
Molybdenum | 0.9 - 1.1 % Show Material materials with Molybdenum of 0.9 - 1.1 % | Quenched and Tempered | ASTM A542 | Plate |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % | Quenched and Tempered | ASTM A542 | Plate |
Phosphorus | 0.025 % Show Material materials with Phosphorus of 0.025 % | Quenched and Tempered | ASTM A542 | Plate |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % | Quenched and Tempered | ASTM A542 | Plate |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % | Quenched and Tempered | ASTM A542 | Plate |
Vanadium | 0.03 % Show Material materials with Vanadium of 0.03 % | Quenched and Tempered | ASTM A542 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |