Nickel Steel
EN 10028-4 Grade 12Ni14 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Ferritischer Edelstahl
DIN 17440 Grade X6Cr17 soft annealed (+A)Ferritischer Edelstahl
DIN 17440 Grade X3CrTi17 soft annealed (+A)Ferritischer Edelstahl
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT)Ferritischer Edelstahl
EN 10028-7 Grade X2CrNi12 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X17CrNi16-2 quenched and tempered (+QT)Martensitischer Edelstahl
SEW 400 Grade X4CrNi13-4 quenched and tempered (+QT1)Martensitischer Edelstahl
SEW 400 Grade X4CrNiMo16-5 quenched and tempered (+QT1)Chromium Molybdenum Steel
EN 10216-2 Grade X12CrMo91 soft annealed (+A)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT2)Martensitischer Edelstahl
DIN 17440 Grade X20Cr13 quenched and tempered (+QT1)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT780)Martensitischer Edelstahl
EN 10272 Grade X3CrNiMo13-4 quenched and tempered (+QT650)Martensitischer Edelstahl
EN 10272 Grade X4CrNiMo16-5-1 quenched and tempered (+QT900)Martensitischer Edelstahl
EN 10272 Grade X4CrNiMo16-5-1 quenched and tempered (+QT760)Martensitischer Edelstahl
DIN 17440 Grade X20CrNi17-2 quenched and tempered (+QT)Ferritischer Edelstahl
DIN 17440 Grade X6CrTi17 soft annealed (+A)Martensitischer Edelstahl
EN 10088-1 Grade X6CrMoS17 soft annealed (+A)Ferritischer Edelstahl
EN 10088-1 Grade X2CrNi12 quenched and tempered (+QT)