EN 10272 Grade X4CrNiMo16-5-1 quenched and tempered (+QT900)

Want to keep this datasheet? Save it now in your required format

Description

The martensitic steel grade X4CrNiMo16-5-1 acc. to DIN EN 10272 : 2001-01is used for hot and cold formed rods for pressure vessels. The material shows favorable corrosion resistance and low-temperature ductility to -200 °C. It also has high corrosion resistance particularly to water, weak acids and bases. oxidizing acids (nitrous acid) and low chloride containing media.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.56 - 7.7 g/cm³

Show Material materials with Density of 7.56 - 7.7 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 - 218 GPa

Show Material materials with Elastic modulus of 200 - 218 GPa

100.0 °C

195 - 213 GPa

Show Material materials with Elastic modulus of 195 - 213 GPa

200.0 °C

185 - 206 GPa

Show Material materials with Elastic modulus of 185 - 206 GPa

300.0 °C

175 - 198 GPa

Show Material materials with Elastic modulus of 175 - 198 GPa

400.0 °C

170 - 190 GPa

Show Material materials with Elastic modulus of 170 - 190 GPa

500.0 °C

180 GPa

Show Material materials with Elastic modulus of 180 GPa

600.0 °C

167 GPa

Show Material materials with Elastic modulus of 167 GPa

700.0 °C

150 GPa

Show Material materials with Elastic modulus of 150 GPa

Elongation

20.0 °C

16 %

Show Material materials with Elongation of 16 %

Elongation, transverse

20.0 °C

14 %

Show Material materials with Elongation, transverse of 14 %

Poisson's ratio

23.0 °C

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Martensitic Stainless Steel

Shear modulus

23.0 °C

77 GPa

Show Material materials with Shear modulus of 77 GPa

Typical for Martensitic Stainless Steel

Tensile strength

20.0 °C

900 - 1100 MPa

Show Material materials with Tensile strength of 900 - 1100 MPa

Tensile strength, transverse

20.0 °C

900 - 1100 MPa

Show Material materials with Tensile strength, transverse of 900 - 1100 MPa

Yield strength Rp0.2

20.0 °C

700 MPa

Show Material materials with Yield strength Rp0.2 of 700 MPa

100.0 °C

660 MPa

Show Material materials with Yield strength Rp0.2 of 660 MPa

150.0 °C

640 MPa

Show Material materials with Yield strength Rp0.2 of 640 MPa

200.0 °C

620 MPa

Show Material materials with Yield strength Rp0.2 of 620 MPa

250.0 °C

600 MPa

Show Material materials with Yield strength Rp0.2 of 600 MPa

300.0 °C

580 MPa

Show Material materials with Yield strength Rp0.2 of 580 MPa

Unlock all property charts

Yield strength Rp0.2, transverse

20.0 °C

700 MPa

Show Material materials with Yield strength Rp0.2, transverse of 700 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

9.9E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.9E-6 1/K

100.0 °C

1.03E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.03E-5 1/K

200.0 °C

1.08E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.08E-5 1/K

300.0 °C

1.12E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.12E-5 1/K

400.0 °C

1.16E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.16E-5 1/K

500.0 °C

1.19E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K

600.0 °C

1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 1/K

700.0 °C

1.24E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.24E-5 1/K

800.0 °C

1.29E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.29E-5 1/K

Unlock all property charts

Max service temperature, long

-200 - 0 °C

Show Material materials with Max service temperature, long of -200 - 0 °C

Melting point

1370 - 1530 °C

Show Material materials with Melting point of 1370 - 1530 °C

Typical for Martensitic Stainless Steel

Specific heat capacity

20.0 °C

430 - 450 J/(kg·K)

Show Material materials with Specific heat capacity of 430 - 450 J/(kg·K)

100.0 °C

482 J/(kg·K)

Show Material materials with Specific heat capacity of 482 J/(kg·K)

200.0 °C

506 J/(kg·K)

Show Material materials with Specific heat capacity of 506 J/(kg·K)

300.0 °C

525 J/(kg·K)

Show Material materials with Specific heat capacity of 525 J/(kg·K)

400.0 °C

547 J/(kg·K)

Show Material materials with Specific heat capacity of 547 J/(kg·K)

500.0 °C

576 J/(kg·K)

Show Material materials with Specific heat capacity of 576 J/(kg·K)

600.0 °C

616 J/(kg·K)

Show Material materials with Specific heat capacity of 616 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

15 - 16 W/(m·K)

Show Material materials with Thermal conductivity of 15 - 16 W/(m·K)

100.0 °C

17.2 W/(m·K)

Show Material materials with Thermal conductivity of 17.2 W/(m·K)

200.0 °C

18.6 W/(m·K)

Show Material materials with Thermal conductivity of 18.6 W/(m·K)

300.0 °C

20 W/(m·K)

Show Material materials with Thermal conductivity of 20 W/(m·K)

400.0 °C

21.2 W/(m·K)

Show Material materials with Thermal conductivity of 21.2 W/(m·K)

500.0 °C

22.3 W/(m·K)

Show Material materials with Thermal conductivity of 22.3 W/(m·K)

600.0 °C

23.3 W/(m·K)

Show Material materials with Thermal conductivity of 23.3 W/(m·K)

700.0 °C

24.1 W/(m·K)

Show Material materials with Thermal conductivity of 24.1 W/(m·K)

800.0 °C

25.5 W/(m·K)

Show Material materials with Thermal conductivity of 25.5 W/(m·K)

900.0 °C

26.9 W/(m·K)

Show Material materials with Thermal conductivity of 26.9 W/(m·K)

1000.0 °C

28.3 W/(m·K)

Show Material materials with Thermal conductivity of 28.3 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

4.7 mm²/s

Show Material materials with Thermal diffusivity of 4.7 mm²/s

100.0 °C

4.5 mm²/s

Show Material materials with Thermal diffusivity of 4.5 mm²/s

200.0 °C

4.5 mm²/s

Show Material materials with Thermal diffusivity of 4.5 mm²/s

300.0 °C

4.6 mm²/s

Show Material materials with Thermal diffusivity of 4.6 mm²/s

400.0 °C

4.4 mm²/s

Show Material materials with Thermal diffusivity of 4.4 mm²/s

500.0 °C

4.1 mm²/s

Show Material materials with Thermal diffusivity of 4.1 mm²/s

600.0 °C

3.6 mm²/s

Show Material materials with Thermal diffusivity of 3.6 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

8E-7 - 9.06E-7 Ω·m

Show Material materials with Electrical resistivity of 8E-7 - 9.06E-7 Ω·m

100.0 °C

9.42E-7 Ω·m

Show Material materials with Electrical resistivity of 9.42E-7 Ω·m

200.0 °C

9.87E-7 Ω·m

Show Material materials with Electrical resistivity of 9.87E-7 Ω·m

300.0 °C

1.03E-6 Ω·m

Show Material materials with Electrical resistivity of 1.03E-6 Ω·m

400.0 °C

1.08E-6 Ω·m

Show Material materials with Electrical resistivity of 1.08E-6 Ω·m

500.0 °C

1.12E-6 Ω·m

Show Material materials with Electrical resistivity of 1.12E-6 Ω·m

600.0 °C

1.18E-6 Ω·m

Show Material materials with Electrical resistivity of 1.18E-6 Ω·m

700.0 °C

1.22E-6 Ω·m

Show Material materials with Electrical resistivity of 1.22E-6 Ω·m

800.0 °C

1.24E-6 Ω·m

Show Material materials with Electrical resistivity of 1.24E-6 Ω·m

900.0 °C

1.26E-6 Ω·m

Show Material materials with Electrical resistivity of 1.26E-6 Ω·m

1000.0 °C

1.27E-6 Ω·m

Show Material materials with Electrical resistivity of 1.27E-6 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.06 %

Show Material materials with Carbon of 0.06 %

Chromium

15 - 17 %

Show Material materials with Chromium of 15 - 17 %

Manganese

1.5 %

Show Material materials with Manganese of 1.5 %

Molybdenum

0.8 - 1.5 %

Show Material materials with Molybdenum of 0.8 - 1.5 %

Nickel

4 - 6 %

Show Material materials with Nickel of 4 - 6 %

Nitrogen

0.02 %

Show Material materials with Nitrogen of 0.02 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.7 %

Show Material materials with Silicon of 0.7 %

Sulfur

0.015 - 0.03 %

Show Material materials with Sulfur of 0.015 - 0.03 %