Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TF00Wrought Copper High Copper Alloy
ASTM B9 Grade C17510 TB00Wrought Copper High Copper Alloy
ASTM B534 Grade C17510 TD04Austenitischer rostfreier Stahl
DIN 17440 Grade X5CrNi18-10 quenched (+Q)Austenitischer rostfreier Stahl
DIN 17440 Grade X5CrNi18-10 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiNb18-10 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X6CrNiNb18-10 quenched (+Q)Austenitischer rostfreier Stahl
EN 10028-7 Grade X5CrNi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X5CrNi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X6CrNiNb18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X3CrNiMoBN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNiNb18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X8CrNiNb16-13 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X5CrNi18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X6CrNiTiB18-10 solution annealed (+AT)