Flexural yield strength: 330 MPa

Quick Comparison

Polyamide 4T (PA4T)

ForTii® K12

Geliefert von:

DSM Engineering Materials

Polyethylenterephthalat (PET)

Arnite® AV2 390

Geliefert von:

DSM Engineering Materials

Polyamide 410 (PA410)

EcoPaXX® Q-DWX10

Geliefert von:

DSM Engineering Materials

Polyamide 410 (PA410)

EcoPaXX® Q-KXG10

Geliefert von:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® Ace MX52

Geliefert von:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® Diablo HDT2700

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Nylatron® GS-51-13

Geliefert von:

DSM Engineering Materials