General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.5 g/cm³ Show Supplier Material materials with Density of 1.5 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | dry | Sim. to ISO 62 |
Water absorption | 5 % Show Supplier Material materials with Water absorption of 5 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | 9.5 GPa Show Supplier Material materials with Elastic modulus of 9.5 GPa | conditioned | ISO 527-1/-2 | |
13 GPa Show Supplier Material materials with Elastic modulus of 13 GPa | dry | ISO 527-1/-2 | ||
Elongation | 2 % Show Supplier Material materials with Elongation of 2 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Elongation of 4 % | conditioned | ISO 527-1/-2 | ||
Flexural modulus | 11.9 GPa Show Supplier Material materials with Flexural modulus of 11.9 GPa | dry | ISO 178 | |
Flexural yield strength | 330 MPa Show Supplier Material materials with Flexural yield strength of 330 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry | ISO 179/1eA |
23 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | dry | ISO 179/1eA | |
23 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m² | conditioned | ISO 179/1eA | |
Tensile strength | 160 MPa Show Supplier Material materials with Tensile strength of 160 MPa | conditioned | ISO 527-1/-2 | |
210 MPa Show Supplier Material materials with Tensile strength of 210 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 1.5e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
8e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Flammability | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Heat deflection temperature | 250 °C Show Supplier Material materials with Heat deflection temperature of 250 °C | dry | ISO 75-1/-2 | 2 MPa | ||
260 °C Show Supplier Material materials with Heat deflection temperature of 260 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Melting point | 260 °C Show Supplier Material materials with Melting point of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 2 mm |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 42% Glass Fiber and MoS2 |