General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density | 1.55 g/cm³ Show Supplier Material materials with Density of 1.55 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 | |
Water absorption | 0.32 % Show Supplier Material materials with Water absorption of 0.32 % | dry | ISO 62 | at 23°C after 24h |
4 % Show Supplier Material materials with Water absorption of 4 % | dry | Sim. to ISO 62 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elastic modulus | -40 °C | 15 GPa Show Supplier Material materials with Elastic modulus of 15 GPa | dry | ISO 527-1/-2 |
14.5 GPa Show Supplier Material materials with Elastic modulus of 14.5 GPa | dry | ISO 527-1/-2 | ||
15.2 GPa Show Supplier Material materials with Elastic modulus of 15.2 GPa | conditioned | ISO 527-1/-2 | ||
40 °C | 14 GPa Show Supplier Material materials with Elastic modulus of 14 GPa | dry, conditioned | ISO 527-1/-2 | |
80 °C | 12.3 GPa Show Supplier Material materials with Elastic modulus of 12.3 GPa | conditioned | ISO 527-1/-2 | |
80 °C | 13.5 GPa Show Supplier Material materials with Elastic modulus of 13.5 GPa | dry | ISO 527-1/-2 | |
100 °C | 8.1 GPa Show Supplier Material materials with Elastic modulus of 8.1 GPa | conditioned | ISO 527-1/-2 | |
100 °C | 13.1 GPa Show Supplier Material materials with Elastic modulus of 13.1 GPa | dry | ISO 527-1/-2 | |
120 °C | 12.8 GPa Show Supplier Material materials with Elastic modulus of 12.8 GPa | dry | ISO 527-1/-2 | |
150 °C | 9.5 GPa Show Supplier Material materials with Elastic modulus of 9.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 8 GPa Show Supplier Material materials with Elastic modulus of 8 GPa | dry | ISO 527-1/-2 | |
180 °C | 6.5 GPa Show Supplier Material materials with Elastic modulus of 6.5 GPa | dry | ISO 527-1/-2 | |
200 °C | 5.9 GPa Show Supplier Material materials with Elastic modulus of 5.9 GPa | dry | ISO 527-1/-2 | |
210 °C | 5.6 GPa Show Supplier Material materials with Elastic modulus of 5.6 GPa | dry | ISO 527-1/-2 | |
Elongation | -40 °C | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | dry | ISO 527-1/-2 |
2.2 % Show Supplier Material materials with Elongation of 2.2 % | conditioned | ISO 527-1/-2 | ||
2.3 % Show Supplier Material materials with Elongation of 2.3 % | dry | ISO 527-1/-2 | ||
40 °C | 2.1 % Show Supplier Material materials with Elongation of 2.1 % | dry | ISO 527-1/-2 | |
40 °C | 2.2 % Show Supplier Material materials with Elongation of 2.2 % | conditioned | ISO 527-1/-2 | |
80 °C | 2.1 % Show Supplier Material materials with Elongation of 2.1 % | dry | ISO 527-1/-2 | |
80 °C | 3.2 % Show Supplier Material materials with Elongation of 3.2 % | conditioned | ISO 527-1/-2 | |
100 °C | 2.3 % Show Supplier Material materials with Elongation of 2.3 % | dry | ISO 527-1/-2 | |
100 °C | 4.8 % Show Supplier Material materials with Elongation of 4.8 % | conditioned | ISO 527-1/-2 | |
120 °C | 2.4 % Show Supplier Material materials with Elongation of 2.4 % | dry | ISO 527-1/-2 | |
150 °C | 3.6 % Show Supplier Material materials with Elongation of 3.6 % | dry | ISO 527-1/-2 | |
160 °C | 4.5 % Show Supplier Material materials with Elongation of 4.5 % | dry | ISO 527-1/-2 | |
180 °C | 5.6 % Show Supplier Material materials with Elongation of 5.6 % | dry | ISO 527-1/-2 | |
200 °C | 6 % Show Supplier Material materials with Elongation of 6 % | dry | ISO 527-1/-2 | |
210 °C | 0.006 % Show Supplier Material materials with Elongation of 0.006 % | dry | ISO 527-1/-2 | |
Flexural modulus | 13.5 GPa Show Supplier Material materials with Flexural modulus of 13.5 GPa | dry | ISO 178 | |
14.2 GPa Show Supplier Material materials with Flexural modulus of 14.2 GPa | conditioned | ISO 178 | ||
120 °C | 12.8 GPa Show Supplier Material materials with Flexural modulus of 12.8 GPa | dry | ISO 178 | |
160 °C | 7.7 GPa Show Supplier Material materials with Flexural modulus of 7.7 GPa | dry | ISO 178 | |
180 °C | 6.1 GPa Show Supplier Material materials with Flexural modulus of 6.1 GPa | dry | ISO 178 | |
200 °C | 5.6 GPa Show Supplier Material materials with Flexural modulus of 5.6 GPa | dry | ISO 178 | |
210 °C | 5.4 GPa Show Supplier Material materials with Flexural modulus of 5.4 GPa | dry | ISO 178 | |
Flexural yield strength | 320 MPa Show Supplier Material materials with Flexural yield strength of 320 MPa | conditioned | ISO 178 | |
330 MPa Show Supplier Material materials with Flexural yield strength of 330 MPa | dry | ISO 178 | ||
120 °C | 260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | dry | ISO 178 | |
160 °C | 165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | dry | ISO 178 | |
180 °C | 135 MPa Show Supplier Material materials with Flexural yield strength of 135 MPa | dry | ISO 178 | |
200 °C | 118 MPa Show Supplier Material materials with Flexural yield strength of 118 MPa | dry | ISO 178 | |
210 °C | 114 MPa Show Supplier Material materials with Flexural yield strength of 114 MPa | dry | ISO 178 | |
Impact strength, Charpy notched | -30 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10.5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | dry | ISO 179/1eA | |
Impact strength, Charpy unnotched | -30 °C | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | dry | ISO 179/1eU | |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 55.0 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m² | dry | ISO 179/1eU | |
Tensile strength | -40 °C | 270 MPa Show Supplier Material materials with Tensile strength of 270 MPa | dry | ISO 527-1/-2 |
220 MPa Show Supplier Material materials with Tensile strength of 220 MPa | conditioned | ISO 527-1/-2 | ||
230 MPa Show Supplier Material materials with Tensile strength of 230 MPa | dry | ISO 527-1/-2 | ||
40 °C | 200 MPa Show Supplier Material materials with Tensile strength of 200 MPa | conditioned | ISO 527-1/-2 | |
40 °C | 210 MPa Show Supplier Material materials with Tensile strength of 210 MPa | dry | ISO 527-1/-2 | |
80 °C | 140 MPa Show Supplier Material materials with Tensile strength of 140 MPa | conditioned | ISO 527-1/-2 | |
80 °C | 190 MPa Show Supplier Material materials with Tensile strength of 190 MPa | dry | ISO 527-1/-2 | |
100 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | conditioned | ISO 527-1/-2 | |
100 °C | 180 MPa Show Supplier Material materials with Tensile strength of 180 MPa | dry | ISO 527-1/-2 | |
120 °C | 165 MPa Show Supplier Material materials with Tensile strength of 165 MPa | dry | ISO 527-1/-2 | |
150 °C | 125 MPa Show Supplier Material materials with Tensile strength of 125 MPa | dry | ISO 527-1/-2 | |
160 °C | 110 MPa Show Supplier Material materials with Tensile strength of 110 MPa | dry | ISO 527-1/-2 | |
180 °C | 95 MPa Show Supplier Material materials with Tensile strength of 95 MPa | dry | ISO 527-1/-2 | |
200 °C | 84 MPa Show Supplier Material materials with Tensile strength of 84 MPa | dry | ISO 527-1/-2 | |
210 °C | 79 MPa Show Supplier Material materials with Tensile strength of 79 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.7e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.7e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
5.4e-07 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5.4e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Glass transition temperature | 160 °C Show Supplier Material materials with Glass transition temperature of 160 °C | dry | ASTM D5026/D7028 | DMTA (tan d) | |
Heat deflection temperature | 320 °C Show Supplier Material materials with Heat deflection temperature of 320 °C | dry | ISO 75-1/-2 | 2 MPa | |
330 °C Show Supplier Material materials with Heat deflection temperature of 330 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Melting point | 335 °C Show Supplier Material materials with Melting point of 335 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Fans & Shrouds, Structural Parts with ForTii® Ace, Carburetor adapter heat shield insulation wall, Cylinder head covers, Instrument panels, Sunroof frame | |
Fillers | 40% Glass Fiber |