Heat deflection temperature, 0.45 MPa: 212 °C

Quick Comparison

Polyetherimid (PEI)

ULTEM™ Resin 2300FC - Americas

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2300F - Americas

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2300R - Asia

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2300R - Americas

Geliefert von:

Sabic

Polyamide 66 (PA66)

Minlon® EFE6096 GY090A

Polyetherimid (PEI)

ULTEM™ Resin 2110EPR - Asia

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2110EPR - Americas

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2300 - Asia

Geliefert von:

Sabic

Polyetherimid (PEI)

ULTEM™ Resin 2300 - Americas

Geliefert von:

Sabic

Polyamide 612 (PA612)

LNP™ LUBRICOMP™ Compound IFL34

Geliefert von:

Sabic

Polybutylenterephthalat (PBT)

LNP™ THERMOCOMP™ Compound WF0039U

Geliefert von:

Sabic