General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 9.3 GPa Show Supplier Material materials with Elastic modulus of 9.3 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 9 GPa Show Supplier Material materials with Flexural modulus of 9 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 227 MPa Show Supplier Material materials with Flexural strength of 227 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Tensile strength | 23.0 °C | 158 MPa Show Supplier Material materials with Tensile strength of 158 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.98E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.98E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature | 210 - 212 °C Show Supplier Material materials with Heat deflection temperature of 210 - 212 °C | ||||
Heat deflection temperature, 0.45 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 180 °C Show Supplier Material materials with Relative temperature index, electrical of 180 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL 746B | |||
Vicat softening temperature | 227 °C Show Supplier Material materials with Vicat softening temperature of 227 °C | ASTM D 1525 | Rate B/50 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236984- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.38mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 1.6- ASTM E 662 <br> UV-light, water exposure/immersion: F1- UL 746C |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
Dielectric strength | 23.0 °C | 24.8 kV/mm Show Supplier Material materials with Dielectric strength of 24.8 kV/mm | ASTM D 149 | in air, 1.6 mm |
Dissipation factor | 23.0 °C | 5.3E-3 [-] Show Supplier Material materials with Dissipation factor of 5.3E-3 [-] | ASTM D 150 | 2450 MHz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
Volume resistivity | 23.0 °C | 3.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 3.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosure/Housing/Cover, Electronics, Enclosures, Furnace/Heater, Fluid Delivery, Gear/Bearing/Slider, Heavy Vehicles, Lab Ware and Clinical Diagnostics, Individual Equiptment, Circuit Protection, Auto Electrical, Auto Aftermarket, Aircraft Exteriors, Animal Testing, Air Conditioning, Aerospace, Aircraft Seating, Air Intake System, Air Cabin Interiors, Defense Vehicles, Document Handling, Data Transfer, Data Management, Building/Construction Sheet, Wiring Devices, Weapon, Wireless Communications, Underhood, Vacuum Cleaner, Plumbing, Pharmaceutical Packaging & Drug Delivery, Power Boat, Pipe/Fitting, Pump, Refrigerator, Security/Detection, Semiconductor, Sail Boat, Sanitary, Surgical Devices, Personal Computing, Non-LED Lighting, Oil/Gas, Motorcycle, Navigation Unit, LED Lighting, Medical Device, Meter Gas, Infrastructure, Interior Rail Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |