General
Property | Temperature | Value | Comment |
---|---|---|---|
Limiting oxygen index | 23.0 °C | 50 % Show Supplier Material materials with Limiting oxygen index of 50 % | |
Relative density | 23.0 °C | 1.51 [-] Show Supplier Material materials with Relative density of 1.51 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.16 % Show Supplier Material materials with Water absorption of 0.16 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 9.3 GPa Show Supplier Material materials with Elastic modulus of 9.3 GPa | ASTM D 638 | 5 mm/min |
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 9 GPa Show Supplier Material materials with Flexural modulus of 9 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 227 MPa Show Supplier Material materials with Flexural strength of 227 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Impact strength, Izod notched | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 85 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 85 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 427 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 427 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 168 MPa Show Supplier Material materials with Tensile strength of 168 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.98E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.98E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature | 210 - 212 °C Show Supplier Material materials with Heat deflection temperature of 210 - 212 °C | ||||
Heat deflection temperature, 0.45 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 180 °C Show Supplier Material materials with Relative temperature index, electrical of 180 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL 746B | |||
Vicat softening temperature | 227 °C Show Supplier Material materials with Vicat softening temperature of 227 °C | ASTM D 1525 | Rate B/50 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥0.25mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 1.6- ASTM E 662 <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.2mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221099- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=470961- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
Dielectric strength | 23.0 °C | 24.8 kV/mm Show Supplier Material materials with Dielectric strength of 24.8 kV/mm | ASTM D 149 | in air, 1.6 mm |
Dissipation factor | 23.0 °C | 5.3E-3 [-] Show Supplier Material materials with Dissipation factor of 5.3E-3 [-] | ASTM D 150 | 2450 MHz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Volume resistivity | 23.0 °C | 3.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 3.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Aircraft Seating, Air Cabin Interiors, Auto Aftermarket, Medical Facility Infrastructure, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 340 to 400.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |