Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 soft annealed (+A)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT2)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT1)Austenitischer rostfreier Stahl
EN 10216-5 Grade X10CrNiMoMnNbVB15-10-1 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10095 Grade X25CrMnNiN25-9-7 solution annealed (+AT)Kohlenstoffarmer Stahl
ASTM A182 Grade F56 Solution-AnnealedAustenitischer rostfreier Stahl
EN 10090 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X53CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10090 Grade X55CrMnNiN20-8 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
EN 10269 Grade X10CrNiMoMnNbVB15-10-1 solution heat-treated and warm worked (+AT+WW)Austenitischer rostfreier Stahl
ASTM A213 Grade TP201 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A213 Grade S21500 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A213 Grade TP202 Heat-TreatedAustenitischer rostfreier Stahl
DIN 17480 Grade X50CrMnNiNbN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
DIN 17480 Grade X53CrMnNiN21-9 solution heat-treated and precipitation hardened (+AT+P)Austenitischer rostfreier Stahl
ASTM A193 Grade B8S Class 1C, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8S Class 1D, Carbide solution treatedAustenitischer rostfreier Stahl
ASTM A193 Grade B8SA Class 1C, Carbide solution treated in the finished condition