Austenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
Sandvik 3R60™ Urea GradeGeliefert von:
Alleima (formerly Sandvik Materials Technology)Austenitischer rostfreier Stahl
UGIMA® 4435 ICH Solution Annealed and Cold drawnGeliefert von:
UgitechAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-5 solution heat-treated and quenchedAustenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMo18-15-4 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 quenched (+Q)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-5 quenched (+Q)Austenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNiMo18-14-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMo18-14-3 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNiSi18-15-4 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMo18-14-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMo18-14-3 quenched (+Q)