Kohlenstoffarmer Stahl
EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10269 Grade 20Mn5 normalized or normalized formed (+N)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X2CrNi19-11 quenched (+Q)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X2CrNiMoN17-13-3 quenched (+Q)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X2CrNiN18-10 quenched (+Q)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X5CrNiMo17-12-2 quenched (+Q)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X6CrNiMoTi17-12-2 quenched (+Q)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X6CrNiTi18-10 quenched (+Q)Kohlenstoffarmer Stahl
EN 10263-2 Grade QSt 38-3 untreated and turnedAustenitischer rostfreier Stahl
DIN 1654-5 Grade X5CrNi18-12 quenched (+Q)