S550QL is a tempered and weldable fine grained steel. yield point: >550 N/mm² application: welded steel constructions of various types, e.g. bridges and load-carrying constructions as well as transport vehicles, lifting and earthmoving machines. application limits: at -40°C is warranted a notch impact energy of 30 J (longitudinal test specimen) cold formability: for nominal size < 16 mm bending radius in transversal direction 3xs in longitudinal direction 4xs (s= nominal thickness) hot forming property: allowed only for stress relieve annealing temperature (max. 580°C) suitability for welding: Steel is weldable according to the common welding methods (EURONORM-INFORMATION Nr. 2 has to be considered)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Typical for Steel

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Steel

Elongation

13.0 %

Show Material materials with Elongation of 13.0 %

Predicted Value, A200

13.4 %

Show Material materials with Elongation of 13.4 %

Predicted Value, A80

16.7 %

Show Material materials with Elongation of 16.7 %

Predicted Value, Transverse

18.4 %

Show Material materials with Elongation of 18.4 %

Predicted Value, A80 Transverse

18.8 %

Show Material materials with Elongation of 18.8 %

Predicted Value, A5

19.9 %

Show Material materials with Elongation of 19.9 %

Predicted Value, A50

20 °C

16 %

Show Material materials with Elongation of 16 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Poisson's ratio

0.3 [-]

Show Material materials with Poisson's ratio of 0.3 [-]

Typical for Steel

Reduction of area

40.1 %

Show Material materials with Reduction of area of 40.1 %

Predicted Value

44.7 %

Show Material materials with Reduction of area of 44.7 %

Predicted Value, Transverse

Shear modulus

79.6 GPa

Show Material materials with Shear modulus of 79.6 GPa

Predicted Value

Shear strength

589.7 MPa

Show Material materials with Shear strength of 589.7 MPa

Predicted Value

Tensile strength

20 °C

590 - 820 MPa

Show Material materials with Tensile strength of 590 - 820 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

590 - 770 MPa

Show Material materials with Tensile strength of 590 - 770 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

640 - 820 MPa

Show Material materials with Tensile strength of 640 - 820 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

640 - 770 MPa

Show Material materials with Tensile strength of 640 - 770 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Yield strength

302.8 MPa

Show Material materials with Yield strength of 302.8 MPa

Predicted Value, RP1

329.7 MPa

Show Material materials with Yield strength of 329.7 MPa

Predicted Value, RP1 Transverse

485.3 MPa

Show Material materials with Yield strength of 485.3 MPa

Predicted Value, Transverse

493 MPa

Show Material materials with Yield strength of 493 MPa

Predicted Value, RP02 Transverse

541.7 MPa

Show Material materials with Yield strength of 541.7 MPa

Predicted Value, RP05

556.5 MPa

Show Material materials with Yield strength of 556.5 MPa

Predicted Value, RP02

623.6 MPa

Show Material materials with Yield strength of 623.6 MPa

Predicted Value, RP002

20 °C

490 MPa

Show Material materials with Yield strength of 490 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

530 MPa

Show Material materials with Yield strength of 530 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

20 °C

550 MPa

Show Material materials with Yield strength of 550 MPa

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Thermal

PropertyValueComment

Coefficient of thermal expansion

11.87 1/K

Show Material materials with Coefficient of thermal expansion of 11.87 1/K

Predicted Value

Specific heat capacity

441.7 J/(kg·K)

Show Material materials with Specific heat capacity of 441.7 J/(kg·K)

Predicted Value

Thermal conductivity

35.68 W/(m·K)

Show Material materials with Thermal conductivity of 35.68 W/(m·K)

Predicted Value

Electrical

PropertyValueComment

Electrical conductivity

5 S/m

Show Material materials with Electrical conductivity of 5 S/m

Predicted Value

Electrical resistivity

35 Ω·m

Show Material materials with Electrical resistivity of 35 Ω·m

Predicted Value

Chemical properties

PropertyValueConditionRelated StandardsShape

Boron

0.005 %

Show Material materials with Boron of 0.005 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Chromium

1.5 %

Show Material materials with Chromium of 1.5 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Copper

0.5 %

Show Material materials with Copper of 0.5 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Manganese

1.7 %

Show Material materials with Manganese of 1.7 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Molybdenum

0.7 %

Show Material materials with Molybdenum of 0.7 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Nickel

2 %

Show Material materials with Nickel of 2 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Niobium

0.06 %

Show Material materials with Niobium of 0.06 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Nitrogen

0.015 %

Show Material materials with Nitrogen of 0.015 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Sulfur

0.01 %

Show Material materials with Sulfur of 0.01 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Vanadium

0.12 %

Show Material materials with Vanadium of 0.12 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Zirconium

0.15 %

Show Material materials with Zirconium of 0.15 %

quenched and tempered (+QT)

EN 10137-2, EN 10025-6

Sheet, Flat

Technological properties

Property
Supplier Disclaimer

The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information.