General
Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel | |||
Elongation | 17.9 % Show Material materials with Elongation of 17.9 % | Predicted Value, A80 | |||
18 % Show Material materials with Elongation of 18 % | Normalized | ASTM A537 | Plate | A200 | |
18.5 % Show Material materials with Elongation of 18.5 % | Predicted Value, Transverse | ||||
19.3 % Show Material materials with Elongation of 19.3 % | Predicted Value, A80 Transverse | ||||
22 % Show Material materials with Elongation of 22 % | Normalized | ASTM A537 | Plate | A50 | |
24.7 % Show Material materials with Elongation of 24.7 % | Predicted Value | ||||
Hardness, Brinell | 239 [-] Show Material materials with Hardness, Brinell of 239 [-] | Predicted Value, Transverse | |||
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | |||
Reduction of area | 40.6 % Show Material materials with Reduction of area of 40.6 % | Predicted Value | |||
43.9 % Show Material materials with Reduction of area of 43.9 % | Predicted Value, Transverse | ||||
Shear modulus | 79.6 GPa Show Material materials with Shear modulus of 79.6 GPa | Predicted Value | |||
Shear strength | 534.1 MPa Show Material materials with Shear strength of 534.1 MPa | Predicted Value | |||
Tensile strength | 450 - 585 MPa Show Material materials with Tensile strength of 450 - 585 MPa | Normalized | ASTM A537 | Plate | |
485 - 620 MPa Show Material materials with Tensile strength of 485 - 620 MPa | Normalized | ASTM A537 | Plate | ||
Yield strength | 264.2 MPa Show Material materials with Yield strength of 264.2 MPa | Predicted Value, RP1 | |||
310 MPa Show Material materials with Yield strength of 310 MPa | Normalized | ASTM A537 | Plate | ||
317.5 MPa Show Material materials with Yield strength of 317.5 MPa | Predicted Value, RP1 Transverse | ||||
338.9 MPa Show Material materials with Yield strength of 338.9 MPa | Predicted Value, RP05 | ||||
345 MPa Show Material materials with Yield strength of 345 MPa | Normalized | ASTM A537 | Plate | ||
345.4 MPa Show Material materials with Yield strength of 345.4 MPa | Predicted Value, Transverse | ||||
378 MPa Show Material materials with Yield strength of 378 MPa | Predicted Value, RP02 | ||||
404.9 MPa Show Material materials with Yield strength of 404.9 MPa | Predicted Value, RP002 | ||||
469.4 MPa Show Material materials with Yield strength of 469.4 MPa | Predicted Value, RP02 Transverse |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 11.94 1/K Show Material materials with Coefficient of thermal expansion of 11.94 1/K | Predicted Value |
Specific heat capacity | 458 J/(kg·K) Show Material materials with Specific heat capacity of 458 J/(kg·K) | Predicted Value |
Thermal conductivity | 32.64 W/(m·K) Show Material materials with Thermal conductivity of 32.64 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.24 % Show Material materials with Carbon of 0.24 % | Normalized | ASTM A537 | Plate |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % | Normalized | ASTM A537 | Plate |
Copper | 0.35 % Show Material materials with Copper of 0.35 % | Normalized | ASTM A537 | Plate |
Manganese | 0.7 - 1.35 % Show Material materials with Manganese of 0.7 - 1.35 % | Normalized | ASTM A537 | Plate |
Molybdenum | 0.08 % Show Material materials with Molybdenum of 0.08 % | Normalized | ASTM A537 | Plate |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % | Normalized | ASTM A537 | Plate |
Phosphorus | 0.025 % Show Material materials with Phosphorus of 0.025 % | Normalized | ASTM A537 | Plate |
Silicon | 0.15 - 0.5 % Show Material materials with Silicon of 0.15 - 0.5 % | Normalized | ASTM A537 | Plate |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % | Normalized | ASTM A537 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |