Kohlenstoffarmer Stahl
DIN 17111 Grade U 7 S 6 hot rolledNickel Chromium Alloy
WL 2.4630 Grade NiCr20Ti soft annealed (+A)Kohlenstoffarmer Stahl
DIN 17111 Grade R 7 S 6 hot rolledMedium Carbon Steel
SEW 101 Grade 49MnVS3 hot worked and controlled cooledMalleable Cast Iron
SAE J158 Grade M3210 AnnealedMalleable Cast Iron
SAE J158 Grade M4504 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5003 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5503 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M7002 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M8501 Liquid quenched and TemperedManganese Steel
SEW 101 Grade 38MnSiVS5 hot worked and controlled cooledWerkzeug- und Maschinenstahl
ISO 4957 Grade 40CrMnMoS8-6Austenitischer rostfreier Stahl
SAE J775 Grade EV-11Medium Carbon Steel
ASTM A234 Grade WPB Heat-TreatedMedium Carbon Steel
ASTM A234 Grade WPC Heat-TreatedMartensitischer Edelstahl
AISI 420F AnnealedMartensitischer Edelstahl
AISI 420F QT800Medium Carbon Steel
ASTM A576 Grade 1145