Streckgrenze Rp 0,2: 427 MPa

Quick Comparison

Nickel Molybdenum Steel

EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-3 Grade P460NH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Unclassified Low Alloy Steel

EN 10028-6 Grade P460QH quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-6 Grade P500QH quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Geliefert von:

3 Matmatch-Lieferanten

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

7000 Serie

AA Standards Grade 7075 T6

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

AA Standards Grade 7075 T651

Geliefert von:

3 Matmatch-Lieferanten

2000 Serie

AA Standards Grade 2024 T3

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

2000 Serie

AA Standards Grade 2024 T81

Geliefert von:

1 Matmatch-Lieferant

2000 Serie

AA Standards Grade 2024 T861

Geliefert von:

1 Matmatch-Lieferant

7000 Serie

AA Standards Grade 7075 T62

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

AA Standards Grade 7075 T652

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

AA Standards Grade 7075 T76

Geliefert von:

3 Matmatch-Lieferanten

Wrought Copper High Copper Alloy

ASTM B534 Grade C17500 TD04

2000 Serie

AA Standards Grade 2024 T851

Geliefert von:

1 Matmatch-Lieferant

Seite 1 von 12