Streckgrenze Rp 0,2: 630 MPa

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Unclassified Low Alloy Steel

EN 10028-6 Grade P690QH quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TF00

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Wrought Copper High Copper Alloy

ASTM B534 Grade C17500 TF00

Wrought Copper High Copper Alloy

ASTM B197 Grade C17300 TH04

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM00 (C72900)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM02 (C72900)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TD02 (C72900)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM02 Strip (C72700)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM04 Strip (C72700)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 96 TM06 Strip (C72700)

Geliefert von:

Materion Brush GmbH

Wrought Copper High Copper Alloy

Alloy 174 (C17410) TH02 Strip

Geliefert von:

Materion Brush GmbH

Wrought Copper High Copper Alloy

ASTM B197 Grade C17300 TF00

Wrought Copper High Copper Alloy

Alloy 190 TM00 (C17200)

Geliefert von:

Materion Brush GmbH
Seite 1 von 9