Austenitischer rostfreier Stahl
Alloy 24 / 1.4565 Solution annealed and quenchedGeliefert von:
Hempel Special MetalsAustenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNiN18-10 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-5 solution heat-treated and quenchedFerritischer Edelstahl
EN 10028-7 Grade X5CrNiN19-9 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X1NiCrMoCuN25-20-7 solution annealed (+AT)Austenitischer rostfreier Stahl
SEW 400 Grade X1NiCrMoCuN25-20-6 quenched (+Q)Austenitischer rostfreier Stahl
SEW 400 Grade X2CrNiMnMoNbN25-18-5-4 quenched (+Q)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr16Ti solution heat-treated and quenchedAustenitischer rostfreier Stahl
ASTM A240 Grade 304LN Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 304N Heat-TreatedNickel Chromium Alloy
DIN 17744 Grade NiCr21Mo6CuNickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr15W solution heat-treated and quenched