EN 10025-2 Grade S355J2 normalized or normalized formed (+N)

View suppliers (85)
Want to keep this datasheet? Save it now in your required format

Description

EN S355J2 is a corrosion resistant, low alloy structural steel, that is known for its good forming properties and high durability. It offers high strength and can be welded to other weldable steels.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

20 °C

7.83 g/cm³

Show Material materials with Density of 7.83 g/cm³

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

-100 °C

217 GPa

Show Material materials with Elastic modulus of 217 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

212 GPa

Show Material materials with Elastic modulus of 212 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

100 °C

207 GPa

Show Material materials with Elastic modulus of 207 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

200 °C

199 GPa

Show Material materials with Elastic modulus of 199 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

300 °C

192 GPa

Show Material materials with Elastic modulus of 192 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

400 °C

184 GPa

Show Material materials with Elastic modulus of 184 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

500 °C

175 GPa

Show Material materials with Elastic modulus of 175 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

600 °C

164 GPa

Show Material materials with Elastic modulus of 164 GPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Elongation

17.7 %

Show Material materials with Elongation of 17.7 %

Predicted Value, A200

19.6 %

Show Material materials with Elongation of 19.6 %

Predicted Value, A50

22.3 %

Show Material materials with Elongation of 22.3 %

Predicted Value, A5

20 °C

12 %

Show Material materials with Elongation of 12 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80 Transverse

20 °C

13 %

Show Material materials with Elongation of 13 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80 Transverse

20 °C

14 %

Show Material materials with Elongation of 14 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80 Transverse

20 °C

14 %

Show Material materials with Elongation of 14 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80

20 °C

15 %

Show Material materials with Elongation of 15 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80 Transverse

20 °C

15 %

Show Material materials with Elongation of 15 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80

20 °C

16 %

Show Material materials with Elongation of 16 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80 Transverse

20 °C

16 %

Show Material materials with Elongation of 16 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80

20 °C

17 %

Show Material materials with Elongation of 17 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80

20 °C

17 %

Show Material materials with Elongation of 17 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Transverse

20 °C

17 %

Show Material materials with Elongation of 17 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

18 %

Show Material materials with Elongation of 18 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

A80

20 °C

18 %

Show Material materials with Elongation of 18 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Transverse

20 °C

18 %

Show Material materials with Elongation of 18 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

19 %

Show Material materials with Elongation of 19 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Transverse

20 °C

20 %

Show Material materials with Elongation of 20 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Transverse

20 °C

20 %

Show Material materials with Elongation of 20 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

21 %

Show Material materials with Elongation of 21 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

22 %

Show Material materials with Elongation of 22 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Hardness, Brinell

243 [-]

Show Material materials with Hardness, Brinell of 243 [-]

Predicted Value, Transverse

Poisson's ratio

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Reduction of area

44.0 %

Show Material materials with Reduction of area of 44.0 %

Predicted Value, Transverse

52.7 %

Show Material materials with Reduction of area of 52.7 %

Predicted Value

Shear modulus

82 GPa

Show Material materials with Shear modulus of 82 GPa

Typical for Low Carbon Steel

Shear strength

513.8 MPa

Show Material materials with Shear strength of 513.8 MPa

Predicted Value

Tensile strength

20 °C

450 - 680 MPa

Show Material materials with Tensile strength of 450 - 680 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

450 - 630 MPa

Show Material materials with Tensile strength of 450 - 630 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

450 - 600 MPa

Show Material materials with Tensile strength of 450 - 600 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

470 - 680 MPa

Show Material materials with Tensile strength of 470 - 680 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

470 - 630 MPa

Show Material materials with Tensile strength of 470 - 630 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

470 - 600 MPa

Show Material materials with Tensile strength of 470 - 600 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

510 - 680 MPa

Show Material materials with Tensile strength of 510 - 680 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

510 - 630 MPa

Show Material materials with Tensile strength of 510 - 630 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

510 - 600 MPa

Show Material materials with Tensile strength of 510 - 600 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Yield strength

243.9 MPa

Show Material materials with Yield strength of 243.9 MPa

Predicted Value, RP1

308.5 MPa

Show Material materials with Yield strength of 308.5 MPa

Predicted Value, RP1 Transverse

367.7 MPa

Show Material materials with Yield strength of 367.7 MPa

Predicted Value, Transverse

379.8 MPa

Show Material materials with Yield strength of 379.8 MPa

Predicted Value, RP05

420.8 MPa

Show Material materials with Yield strength of 420.8 MPa

Predicted Value, RP02

477.7 MPa

Show Material materials with Yield strength of 477.7 MPa

Predicted Value, RP02 Transverse

480.2 MPa

Show Material materials with Yield strength of 480.2 MPa

Predicted Value, RP002

20 °C

265 MPa

Show Material materials with Yield strength of 265 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

275 MPa

Show Material materials with Yield strength of 275 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

285 MPa

Show Material materials with Yield strength of 285 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

295 MPa

Show Material materials with Yield strength of 295 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

315 MPa

Show Material materials with Yield strength of 315 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

325 MPa

Show Material materials with Yield strength of 325 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

335 MPa

Show Material materials with Yield strength of 335 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

345 MPa

Show Material materials with Yield strength of 345 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

355 MPa

Show Material materials with Yield strength of 355 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

100 °C

194 - 254 MPa

Show Material materials with Yield strength of 194 - 254 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

194 - 249 MPa

Show Material materials with Yield strength of 194 - 249 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

194 - 234 MPa

Show Material materials with Yield strength of 194 - 234 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

194 - 224 MPa

Show Material materials with Yield strength of 194 - 224 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

194 - 214 MPa

Show Material materials with Yield strength of 194 - 214 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

194 MPa

Show Material materials with Yield strength of 194 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

214 - 254 MPa

Show Material materials with Yield strength of 214 - 254 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

214 - 249 MPa

Show Material materials with Yield strength of 214 - 249 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

214 - 234 MPa

Show Material materials with Yield strength of 214 - 234 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

214 - 224 MPa

Show Material materials with Yield strength of 214 - 224 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

214 MPa

Show Material materials with Yield strength of 214 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

224 - 254 MPa

Show Material materials with Yield strength of 224 - 254 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

224 - 249 MPa

Show Material materials with Yield strength of 224 - 249 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

224 - 234 MPa

Show Material materials with Yield strength of 224 - 234 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

224 MPa

Show Material materials with Yield strength of 224 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

234 - 254 MPa

Show Material materials with Yield strength of 234 - 254 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

234 - 249 MPa

Show Material materials with Yield strength of 234 - 249 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

234 MPa

Show Material materials with Yield strength of 234 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

249 - 254 MPa

Show Material materials with Yield strength of 249 - 254 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

249 MPa

Show Material materials with Yield strength of 249 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

100 °C

254 MPa

Show Material materials with Yield strength of 254 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

166 - 226 MPa

Show Material materials with Yield strength of 166 - 226 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

166 - 221 MPa

Show Material materials with Yield strength of 166 - 221 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

166 - 206 MPa

Show Material materials with Yield strength of 166 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

166 - 196 MPa

Show Material materials with Yield strength of 166 - 196 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

166 - 186 MPa

Show Material materials with Yield strength of 166 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

166 MPa

Show Material materials with Yield strength of 166 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

186 - 226 MPa

Show Material materials with Yield strength of 186 - 226 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

186 - 221 MPa

Show Material materials with Yield strength of 186 - 221 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

186 - 206 MPa

Show Material materials with Yield strength of 186 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

186 - 196 MPa

Show Material materials with Yield strength of 186 - 196 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

186 MPa

Show Material materials with Yield strength of 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

196 - 226 MPa

Show Material materials with Yield strength of 196 - 226 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

196 - 221 MPa

Show Material materials with Yield strength of 196 - 221 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

196 - 206 MPa

Show Material materials with Yield strength of 196 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

196 MPa

Show Material materials with Yield strength of 196 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

206 - 226 MPa

Show Material materials with Yield strength of 206 - 226 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

206 - 221 MPa

Show Material materials with Yield strength of 206 - 221 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

206 MPa

Show Material materials with Yield strength of 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

221 - 226 MPa

Show Material materials with Yield strength of 221 - 226 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

221 MPa

Show Material materials with Yield strength of 221 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

200 °C

226 MPa

Show Material materials with Yield strength of 226 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

146 - 206 MPa

Show Material materials with Yield strength of 146 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

146 - 202 MPa

Show Material materials with Yield strength of 146 - 202 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

146 - 186 MPa

Show Material materials with Yield strength of 146 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

146 - 176 MPa

Show Material materials with Yield strength of 146 - 176 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

146 - 166 MPa

Show Material materials with Yield strength of 146 - 166 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

146 MPa

Show Material materials with Yield strength of 146 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

166 - 206 MPa

Show Material materials with Yield strength of 166 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

166 - 186 MPa

Show Material materials with Yield strength of 166 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

166 MPa

Show Material materials with Yield strength of 166 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

166 - 202 MPa

Show Material materials with Yield strength of 166 - 202 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

166 - 176 MPa

Show Material materials with Yield strength of 166 - 176 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

176 - 206 MPa

Show Material materials with Yield strength of 176 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

176 - 202 MPa

Show Material materials with Yield strength of 176 - 202 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

176 - 186 MPa

Show Material materials with Yield strength of 176 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

176 MPa

Show Material materials with Yield strength of 176 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

186 - 206 MPa

Show Material materials with Yield strength of 186 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

186 MPa

Show Material materials with Yield strength of 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

186 - 202 MPa

Show Material materials with Yield strength of 186 - 202 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

202 - 206 MPa

Show Material materials with Yield strength of 202 - 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

202 MPa

Show Material materials with Yield strength of 202 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

250 °C

206 MPa

Show Material materials with Yield strength of 206 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

126 - 186 MPa

Show Material materials with Yield strength of 126 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

126 - 181 MPa

Show Material materials with Yield strength of 126 - 181 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

126 - 166 MPa

Show Material materials with Yield strength of 126 - 166 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

126 - 156 MPa

Show Material materials with Yield strength of 126 - 156 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

126 - 146 MPa

Show Material materials with Yield strength of 126 - 146 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

126 MPa

Show Material materials with Yield strength of 126 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

146 - 186 MPa

Show Material materials with Yield strength of 146 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

146 - 166 MPa

Show Material materials with Yield strength of 146 - 166 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

146 MPa

Show Material materials with Yield strength of 146 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

146 - 181 MPa

Show Material materials with Yield strength of 146 - 181 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

146 - 156 MPa

Show Material materials with Yield strength of 146 - 156 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

156 - 186 MPa

Show Material materials with Yield strength of 156 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

156 - 181 MPa

Show Material materials with Yield strength of 156 - 181 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

156 - 166 MPa

Show Material materials with Yield strength of 156 - 166 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

156 MPa

Show Material materials with Yield strength of 156 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

166 - 186 MPa

Show Material materials with Yield strength of 166 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

166 MPa

Show Material materials with Yield strength of 166 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

166 - 181 MPa

Show Material materials with Yield strength of 166 - 181 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

181 - 186 MPa

Show Material materials with Yield strength of 181 - 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

181 MPa

Show Material materials with Yield strength of 181 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

300 °C

186 MPa

Show Material materials with Yield strength of 186 MPa

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

-100 °C

1.08e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.08e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

1.19e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.19e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

100 °C

1.25e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.25e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

200 °C

1.3e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.3e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

300 °C

1.36e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.36e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

400 °C

1.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.41e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

500 °C

1.45e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.45e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

600 °C

1.49e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.49e-05 1/K

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Max service temperature

305.4 °C

Show Material materials with Max service temperature of 305.4 °C

Predicted Value, Long

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Specific heat capacity

-100 °C

423 J/(kg·K)

Show Material materials with Specific heat capacity of 423 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

461 J/(kg·K)

Show Material materials with Specific heat capacity of 461 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

100 °C

479 J/(kg·K)

Show Material materials with Specific heat capacity of 479 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

200 °C

499 J/(kg·K)

Show Material materials with Specific heat capacity of 499 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

300 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

400 °C

536 J/(kg·K)

Show Material materials with Specific heat capacity of 536 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

500 °C

558 J/(kg·K)

Show Material materials with Specific heat capacity of 558 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

600 °C

587 J/(kg·K)

Show Material materials with Specific heat capacity of 587 J/(kg·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Thermal conductivity

-100 °C

37.6 W/(m·K)

Show Material materials with Thermal conductivity of 37.6 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

42.2 W/(m·K)

Show Material materials with Thermal conductivity of 42.2 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

100 °C

43.2 W/(m·K)

Show Material materials with Thermal conductivity of 43.2 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

200 °C

42.9 W/(m·K)

Show Material materials with Thermal conductivity of 42.9 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

300 °C

41.2 W/(m·K)

Show Material materials with Thermal conductivity of 41.2 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

400 °C

39.1 W/(m·K)

Show Material materials with Thermal conductivity of 39.1 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

500 °C

36.6 W/(m·K)

Show Material materials with Thermal conductivity of 36.6 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

600 °C

34.1 W/(m·K)

Show Material materials with Thermal conductivity of 34.1 W/(m·K)

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Thermal diffusivity

-100 °C

12.9 mm²/s

Show Material materials with Thermal diffusivity of 12.9 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

11.7 mm²/s

Show Material materials with Thermal diffusivity of 11.7 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

100 °C

11.2 mm²/s

Show Material materials with Thermal diffusivity of 11.2 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

200 °C

10.3 mm²/s

Show Material materials with Thermal diffusivity of 10.3 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

300 °C

9.4 mm²/s

Show Material materials with Thermal diffusivity of 9.4 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

400 °C

8.3 mm²/s

Show Material materials with Thermal diffusivity of 8.3 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

500 °C

7.1 mm²/s

Show Material materials with Thermal diffusivity of 7.1 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

600 °C

5.7 mm²/s

Show Material materials with Thermal diffusivity of 5.7 mm²/s

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Electrical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Electrical conductivity

7 S/m

Show Material materials with Electrical conductivity of 7 S/m

Predicted Value

Electrical resistivity

-100 °C

1.82e-07 Ω·m

Show Material materials with Electrical resistivity of 1.82e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

20 °C

2.47e-07 Ω·m

Show Material materials with Electrical resistivity of 2.47e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

100 °C

2.96e-07 Ω·m

Show Material materials with Electrical resistivity of 2.96e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

200 °C

3.68e-07 Ω·m

Show Material materials with Electrical resistivity of 3.68e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

300 °C

4.55e-07 Ω·m

Show Material materials with Electrical resistivity of 4.55e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

400 °C

5.56e-07 Ω·m

Show Material materials with Electrical resistivity of 5.56e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

500 °C

6.75e-07 Ω·m

Show Material materials with Electrical resistivity of 6.75e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

600 °C

8.13e-07 Ω·m

Show Material materials with Electrical resistivity of 8.13e-07 Ω·m

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Magnetic

PropertyValueComment

Curie temperature

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValueConditionRelated StandardsShape

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Copper

0.55 %

Show Material materials with Copper of 0.55 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Manganese

1.6 %

Show Material materials with Manganese of 1.6 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Phosphorus

0.025 %

Show Material materials with Phosphorus of 0.025 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Silicon

0.55 %

Show Material materials with Silicon of 0.55 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %

normalized or normalized formed (+N)

EN 10025-2, EN 10025

Strip, Sheet, Flat, Rod, Wire

Technological properties

Property
Supplier Disclaimer

The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information.

Do you have a technical question or need more information about this material?

Post it as a comment below and receive answers from engineers and other community members.