Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.71 g/cm³ Show Supplier Material materials with Dichte of 8.71 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 8 % Show Supplier Material materials with Dehnung A5 of 8 % | |
Elastizitätsmodul | 23.0 °C | 131 GPa Show Supplier Material materials with Elastizitätsmodul of 131 GPa | |
Flächenreduzierung | 23.0 °C | 18 % Show Supplier Material materials with Flächenreduzierung of 18 % | |
Härte, HBW | 23.0 °C | 210 [-] Show Supplier Material materials with Härte, HBW of 210 [-] | HBW 10/3000 |
Härte, Rockwell B | 23.0 °C | 95 [-] Show Supplier Material materials with Härte, Rockwell B of 95 [-] | |
Streckgrenze Rp0,5 | 23.0 °C | 475 MPa Show Supplier Material materials with Streckgrenze Rp0,5 of 475 MPa | |
Zugfestigkeit | 23.0 °C | 544 MPa Show Supplier Material materials with Zugfestigkeit of 544 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 380 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 208 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 208 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.80E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.80E+7 S/m |
Specific Electrical conductivity | 48 % IACS Show Supplier Material materials with Specific Electrical conductivity of 48 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | AMPCOLOY® 940 is used wherever a good electrical or thermal conductivity is required together with high mechanical properties: Electrode holders, parts for energy engineering |