Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 6.93 g/cm³ Show Supplier Material materials with Dichte of 6.93 g/cm³ |
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Druckfestigkeit | 23.0 °C | 1551 MPa Show Supplier Material materials with Druckfestigkeit of 1551 MPa | |
Druckfestigkeit, 0,1% | 23.0 °C | 689 MPa Show Supplier Material materials with Druckfestigkeit, 0,1% of 689 MPa | |
Elastizitätsmodul | 23.0 °C | 110 GPa Show Supplier Material materials with Elastizitätsmodul of 110 GPa | |
Härte, HBW | 23.0 °C | 375 [-] Show Supplier Material materials with Härte, HBW of 375 [-] | HBW 10/3000 |
Härte, Rockwell C | 23.0 °C | 40 [-] Show Supplier Material materials with Härte, Rockwell C of 40 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.62E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 420 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 33 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 33 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 4.00E+6 S/m |
Specific Electrical conductivity | 8 % IACS Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS |
Chemical properties
Property | Value |
---|---|
Kupfer | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | The phenomenal success of this alloy led to its use as forming rolls, bending and wiping blocks and it is considered the standard material in this field of applications. Due to its inherent friction properties, this alloy has an excellent behaviour in any wear application where high compression loads are present. |