Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.54 g/cm³ Show Supplier Material materials with Dichte of 1.54 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.3 % Show Supplier Material materials with Wasserabsorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 8.5 GPa Show Supplier Material materials with Elastizitätsmodul of 8.5 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 30 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 30 kJ/m² | dry | ISO 179/1eU |
23 °C | 30 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 30 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 215 °C Show Supplier Material materials with Ball pressure temperature of 215 °C | dry | IEC 60695-10-2 | |||
Entflammbarkeit | V-2 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 2 mm | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.75 mm | ||
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 550 V Show Supplier Material materials with Kriechstromfestigkeit of 550 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 250 °C | 18 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 18 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | dry | Sim. to ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Residual Current Breaker with Overload, Motor Starter/Overload Relays | |
Certifications | Yellow Card Available | |
Fillers | 25% Glass Fiber |