Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.62 g/cm³ Show Supplier Material materials with Dichte of 1.62 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Wasserabsorption | 4 % Show Supplier Material materials with Wasserabsorption of 4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.7 % Show Supplier Material materials with Dehnung of 2.7 % | dry, conditioned | ISO 527-1/-2 | |
Elastizitätsmodul | 17 GPa Show Supplier Material materials with Elastizitätsmodul of 17 GPa | dry, conditioned | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry | ISO 179/1eA |
Zugfestigkeit | 275 MPa Show Supplier Material materials with Zugfestigkeit of 275 MPa | dry, conditioned | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glasübergangstemperatur | 130 °C Show Supplier Material materials with Glasübergangstemperatur of 130 °C | dry | ASTM D5026/D7028 | DMTA (tan d) | |
Schmelzpunkt | 315 °C Show Supplier Material materials with Schmelzpunkt of 315 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 2 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |